BAROT-06812
ActiveIndium Corporation of America
SAC0307 TRIANGLE BAR

BAROT-06812
ActiveIndium Corporation of America
SAC0307 TRIANGLE BAR
Description
General part information
BAROT-06812
SAC0307 TRIANGLE BAR
Technical Specifications
Parameters and characteristics for this part
| Specification | BAROT-06812 |
|---|---|
| Ag Composition | 0.3 % |
| Composition Elements | Cu, Ag, Sn |
| Composition Formula | Sn99Cu0.7Ag0.3 |
| Cu Composition | 0.7 % |
| Melting Point | 441 °F |
| Sn Composition | 99 % |
| Storage/Refrigeration Temperature (Maximum) | 104 °F |
| Storage/Refrigeration Temperature (Minimum) | 50 °F |
| Type | Bar Solder |